An aluminium truss bottom chord in tension, designed to China's GB 50429, checks net section capacity at its bolted connection — the same gross-versus-net-section distinction discussed for the CSA S157 aluminium tension chord example covered elsewhere in this series, confirmed here under an independently developed code.

Every check above runs automatically inside the Structyze Aluminium Truss Member module — this particular module is part of the full desktop catalogue rather than the free browser trial, since the trial only carries a curated flagship set. You can still try the free trial modules right now to see the same calculation style in action on RCC Beam, Column, Slab and a handful of others.

The Example We'll Use

  • Bottom chord: aluminium alloy 6061-T6, flat bar 90 mm × 8 mm, bolted connection with 2-14 mm bolts
  • f_y: 240 MPa, f_u: 290 MPa
  • Design tension force: 118 kN

Working Through It

Gross section yield check: design yield resistance = (240/1.1) × (90 × 8) × 10⁻³ = 157 kN. Utilization: 118/157 = 0.75.

Net section fracture check, with bolt holes (14 mm plus clearance, 16 mm effective) removing material: A_n = (90 − 2 × 16) × 8 = 464 mm².

Net section fracture resistance: (290/1.25) × 464 × 10⁻³ = 107.6 kN.

Utilization at the net section: 118/107.6 = 1.10 — this chord fails at its bolted connection despite the gross section clearing comfortably.

What Governs, and Why

Net section fracture at the bolt holes governs and fails at utilization 1.10, despite the gross section yield check clearing at a comfortable 0.75 — paralleling the CSA S157 example elsewhere in this series, confirming once again that an aluminium tension member's connection, not its unperforated length, is frequently the real governing location, and needs its own explicit net section check rather than relying on a gross section pass alone.

Where Structyze Takes Over

Every check above runs automatically inside the Structyze Aluminium Truss Member module — this particular module is part of the full desktop catalogue rather than the free browser trial, since the trial only carries a curated flagship set. You can still try the free trial modules right now to see the same calculation style in action on RCC Beam, Column, Slab and a handful of others.

For Aluminium Truss Member and the rest of the full catalogue — 80+ components across RCC, Steel, Composite, Timber, Masonry and more, across 20+ design codes — buy the full Structyze desktop app or see everything it does on the Software page.

Quick FAQ

Why does this chord's net section check fail more decisively than the CSA S157 example elsewhere in this series?

The specific margin depends on each example's particular combination of plate width, bolt diameter, and applied force — this example's narrower 90 mm bar width relative to its bolt diameter removes a proportionally larger share of the cross-section at the connection, producing a more decisive net section shortfall than the CSA S157 example's own proportions showed.

Would using a single larger bolt instead of two smaller ones improve this connection's net section capacity?

Potentially, if the larger bolt's hole removes less total width than the two smaller holes combined, though this trade-off needs checking against the single bolt's own shear and bearing capacity to confirm it can still carry the full connection force without introducing a different governing limit.

Final Thoughts

A second independent code reaching the same conclusion as the CSA S157 example elsewhere in this series — an aluminium tension chord's bolted connection, not its gross cross-section, is exactly where the real governing check most often lives, and skipping the net section verification is how that governing limit gets missed.